Calcium silicate at 250 °C — heat-loss table

λ = 0.067 W/m·K at mean temperature ((250+20)/2 = 135 °C, from the published curve). Pipe losses per metre, four thicknesses, savings vs bare.

Pipe30 mm W/m50 mm W/m80 mm W/m100 mm W/mBARE W/mSurface @50 mmSaving €/m·yr @50 mmt CO2/m·yr
DN258265534824135 °C€860.32
DN5012091716443638 °C€1680.62
DN80159117897964240 °C€2560.94
DN1001931391049182641 °C€3351.23
DN1502651861361171,21642 °C€5021.84
DN2003322301651411,58343 °C€6602.42
DN3004703202241902,34044 °C€9863.61

Assumptions: 20 °C ambient, still air (h=10 W/m²·K combined), €0.05/kWh fuel, 8000 h/yr, 82% efficiency, 0.183 kg CO2e/kWh (DESNZ 2024). Flat surfaces at this duty: bare 2,300 W/m² → 270 W/m² at 50 mm (≈€990/m²·yr saved). Method: ASTM C680 simplified — methodology. Your exact case: free calculator.

Context

All materials at 250 °C

Materialλ W/m·KLoss W/mSurfaceSaving €/m·yrt CO2/m·yr
Stone wool (mineral wool)0.05211237 °C€3481.3
Glass wool0.05010636 °C€3511.3
Ceramic fibre (RCF / AES blanket)0.06012739 °C€3411.2
Aerogel blanket0.0276129 °C€3731.4
Calcium silicate0.06713941 °C€3351.2
Expanded perlite0.07014542 °C€3321.2
Cellular glass0.05812238 °C€3431.3
Microporous (fumed-silica) panels0.0235027 °C€3781.4
E-glass needle mat0.05010636 °C€3511.3
Silica needle mat / fabric0.05511737 °C€3461.3

DN100 pipe at 250 °C, 50 mm insulation, per metre of pipe; bare loss 826 W/m. λ at mean temperature; € and CO2 per metre·year at €0.05/kWh, 8000 h, 82% efficiency. Method: ASTM C680 simplified (h=10).

Material datasheet: Calcium silicate → · temperature class: by temperature →

FAQ

Questions on this topic

How much heat does a pipe at 250 °C lose with calcium silicate?
With 50 mm at 250 °C (λ=0.067 at mean): DN50 loses 91 W/m, DN100 139 W/m, DN200 230 W/m — vs 826 W/m bare for DN100. Full table on this page.
What surface temperature does calcium silicate give at 250 °C?
≈41 °C with 50 mm on DN100 (20 °C ambient, still air). Personnel-protection targets (≤45–60 °C) may need more thickness — see the 80/100 mm columns.